AWS A5.11 / ASME SFA5.11 ENiCrMo-4
Applications
Welding of UNS 10276, overlay cladding of low alloy or carbon steel
Characteristics on Usage
Notes on Usage
Welding Position(All-Position) Current
provides general corrosion resistance and due to the high molybdenum content, a strong resistance to stress corrosion cracking, pitting and crevice corrosion.
① Dry the electrodes at 350℃(662℉) for 60 minutes before use.
② Keep the current as low as possible and length as short as possible.
③ Remove rust, water, oil and paint from the groove.
AC or DC+