AWS A5.5 / ASME SFA5.5 E10016-G
JIS Z3211 E6916-N4CM1 U
EN 757 - E55 0 B 1 2
Notes on Usage
Welding Positions:
① Dry the electrodes at 350~400℃(662~752℉) for 60 minutes before use.
② Adopt back step method or strike the arc on a small steel plate prepared for this particular purpose.
③ Preheat at 100~150℃(212~302℉). The temperature varies in accordance with plate thickness and kind of steel.
Applications
AWS A5.5 / ASME SFA5.5 E10016-G can be used for welding of high tensile steel, such as pressure vessels, penstock and bridges.
Welding Position
Characteristics on Usage
·Its workability and X-ray properties are superb in all positions.
·Good toughness of all-weld metal.
·Extremely low hydrogen contents and good crack resistibility.
Current
AC or DC +