AWS A 5.17 F7A8-EM12K welding fulx xiang welding is a high—basic agglomerated submerged arc flux. It is suitable for using DC+ single, AC single, DC+/AC and AC/AC. It provides excellent weld ability even in narrow groove. Due to its neutral behavior, good mechanical properties of weld metal can be controlled by using the appropriate wire grade.
With combination of low phosphorus wires (TSW-E22R or TSW-E23R), the X and J factors can be controlled to satisfy the step cooling requirement.
Heat treatable and heat resistant low-alloy CrMo steel Pressure vessel Fine grain structural steels for low temperature requirements High tensile fine grain steels
AWS A 5.17 F7A8-EM12K
EN ISO14171-A S38 6 FB S2Si
Characteristics and Application
Typical chemical Composition of Weld Metal (%)
Welding Positions:
Notes on usage:
1. Dry the flux at 300-350℃ for 2—4hr holding time.
2. Adding proper quantity of new flux with the used one to maintain good quality of weld metal.
Mechanical Properties
Welding Flux
Yield strength 416Mpa Tensile Strenght 489MPa Elongation 34% Charpy V-Notch -62℃ 111J
C 0.06 Mn 1.08 Si 0.40 P 0.018 S 0.004 Cr 0.020 Mo 0.020 Cu 0.046