JIS Z3251 DF2A-300-B
Notes on Usage
Welding Positions:
1. Preheating is unnecessary, in general, in case of multi-layer welding
of low alloy steel and high carbon steel, preheat at about
150℃(302℉).
2. Adopt back step method or strike arc on al small steel plate prepared
for this particular purpose for preventing blow hole at the arc starting.
3. Dry the electrodes at 350~400℃(662~752℉) for 60 minutes before
use.
Applications
JIS Z3251 DF2A-300-B. For intermetallic light abrasion, hardfacing and repairing of worn parts of shafts, gears, wheels, etc.
Characteristics on Usage
Stable arc. Beautiful bead appearance. Good flow and easy removal of the slag. High abrasion resistance and impact resistance.
Typical Chemical Composition of All-weld Metal(wt%)
Typical Mechanical Properties of All-Weld Metal
Available sizes and Recommended Current