AWS: ERNi-CI Stainless welding wire For cast iron joining and repair
DETAILS
Welding Positions
Welding Positions
WIRE COMPOSITION
Features
Welds produced are generally more machinable than a Tech-Rod® 55 deposit
A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
Certificate showing actual wire composition available online
Typical Applications
Used for welding of cast irons to other cast irons as well as for joining cast irons to mild steels and stainless steels
Readily used for the repair of castings
Maintenance and Repair
All
Shielding Gas
100% Argon
CONFORMANCE
CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.14 ERNi-CI